設計 · ガラス構造
ガラスたわみの使用性検定比 (EN 16612)
EN 16612 第9項によるガラス板の使用限界状態たわみ検定比: ηw = w / wlim.
Catalog formula, not a design. Check input values, coefficients, and limits against the standard and its national annex.
Formula and quantities
| Symbol | Name | Unit | Note |
|---|---|---|---|
| 計算されたガラス板のたわみ | mm | ||
| 許容たわみ限界 | mm | ||
| たわみ検定比 (<= 1.0) | 1 | Result |
例題
= 6.6 mm · = 12 mm
= 0.55
Standard and source
- Standard
- EN 16612:2019
- Result
- in 1
Reference to clause and equation, no standard text. The description is written in our own words.
Try it
Continue with Mia
Fills the input field in CALC; nothing is sent until you send it.
No matching formula yet? Find the right calculation rule.
Describe what you want to determine. Mia searches the formula catalog first and clarifies assumptions before anything is calculated.
検索は設計 › ガラス構造で開始されます。
Miaknows the formula catalog and asks for what is missing.