設計 · アルミ構造

HAZ低減引張強さ fu,haz

  • タイプ:特性値
  • バージョン1
  • 2026/11/13にレビュー済み

溶接部近傍の熱影響部(HAZ)における低減引張強さ: fu,haz = ρu,haz · fu。

fu,haz=ρu,haz⋅fu\displaystyle f_{u,haz} = \rho _{u,haz} \cdot f_{u}
Apply in CALC

Catalog formula, not a design. Check input values, coefficients, and limits against the standard and its national annex.

Formula and quantities

SymbolNameUnitNote
ρu,haz\displaystyle \rho_{u,haz}引張強さに対するHAZ軟化係数1
fu\displaystyle f_{u}母材の特性引張強さN/m²
fu,haz\displaystyle f_{u,haz}HAZ低減引張強さN/m²Result

例題

ρu,haz\displaystyle \rho_{u,haz} = 0.6 · fu\displaystyle f_{u} = 310,000,000 N/m²

fu,haz\displaystyle f_{u,haz} = 186,000,000 N/m²

Standard and source

Result
fu,haz\displaystyle f_{u,haz} in MPa

Reference to clause and equation, no standard text. The description is written in our own words.

Try it

Unit system
fu,haz\displaystyle f_{u,haz} = 186,000,000 N/m²= (0.6 1) · (310,000,000 N/m²)

Continue with Mia

Fills the input field in CALC; nothing is sent until you send it.

No matching formula yet? Find the right calculation rule.

Describe what you want to determine. Mia searches the formula catalog first and clarifies assumptions before anything is calculated.

検索は設計 › アルミ構造で開始されます。

Miaknows the formula catalog and asks for what is missing.

You clarify missing information with Mia in the next step. Nothing is calculated yet.